Explanation: hot spots are the thick sections, those cool slower than other sections causing abnormal shrinkage. defects such as voids cracks and porosity are created at these hot spots.
Q. Defects caused by the chilling of the casting are known as?
β
Correct Answer: (A)
hot spots
Explanation by: Mr. Dubey
hot spots are the thick sections, those cool slower than other sections causing abnormal shrinkage. defects such as voids cracks and porosity are created at these hot spots.