Q. Spurious indications might be caused by which of the following?

  • (A) Mode conversion from beam spread in a long specimen
  • (B) Surface waves generated during straight beam testing
  • (C) A test piece with a smooth machined surface
  • (D) All of the above
πŸ’¬ Discuss
βœ… Correct Answer: (A) Mode conversion from beam spread in a long specimen